Figure 8.

SEM micrographs of Ni-Pd on the foam surface, obtained after reduction of chloride precursors at 533 K, Ni loading: (a) 5 wt% and (b) 20 wt%.

SEM micrographs of Ni-Pd on the foam surface, obtained after reduction of chloride precursors at 533 K, Ni loading: (a) 5 wt% and (b) 20 wt%.