Experimental data and corresponding theoretical strain-time curves (a) and maximum contracted strains (b) for PLA strips at building speed varying from 10 to 150 mm s−1. All of the strips contract after heating and the maximum contract strain is almost linear to the building speed from 30 to 120 mm s−1.