. 2015 Mar 13;5:9089. doi: 10.1038/srep09089

Figure 3.

Figure 3

(a) Change of capacitance normalized to the capacitance at zero magnetic field vs. magnetic field for the superlattice and 20 nm thick BFO film. (b) In-plane resistance of the superlattice and the 20 nm thick BFO film vs. magnetic field. For 10 K and μ0H = 0 T, the resistivity of the superlattice sample is (7.5 ± 0.3) × 105 Ωcm and (1.1 ± 0.1) × 106 Ωcm for the thick BFO film.