Skip to main content
. 2015 Mar 12;6:720–725. doi: 10.3762/bjnano.6.73

Figure 3.

Figure 3

Typical XRD patterns of the ZnO nanorod arrays grown at 95 °C for 3 h on (a) Si, (b) PET and (c) glass substrates, respectively.