Figure 6.

Figure 6

Microstructures of 63s scaffolds with 10 wt.% HANw ((a) low and (b) high magnified image) and 10 wt.% HANp ((d) low and (e) high magnified image) after immersion in SBF for 7 days: (a) low and (b) high magnified image. EDS of the mineral layer ((c) 63s glass/HANw scaffolds; (f) 63s glass/HANp scaffolds).