Impact of the polymeric binder solution on the performance of the GMR sensors printed on the FPC. The size of the GMR flakes is 150 μm; the concentration of the GMR powder in the binder is 90%. a) Magnetoelectric performance of the sensors. b) Summary of the maximum achievable GMR ratio (green bar) and operation temperature (red bar) for the sensors prepared by mixing the GMR powder with binder solutions based on different polymers.