Skip to main content
. 2014 Nov 4;27(5):880–885. doi: 10.1002/adma.201403907

Figure 4.

Figure 4

a) Comparison of the GMR performance of the printed sensors with a size of flakes of 36 and 150 μm dispersed in PCH binder solution. b) The GMR response of the sensors with the concentration of the GMR powder in the binder solution. The size of flakes is 36 μm; PCH polymer is used for the binder solution.