(A) Current-time response curve for successive injection of H2O2 at Pt-Au/rGSs/GCE measured at 0 V. Inset: Magnified image of the region in the rectangle; (B) Calibration curves of response current vs. H2O2 concentration at Pt-Au/rGSs/GCE.