Skip to main content
. Author manuscript; available in PMC: 2016 Mar 1.
Published in final edited form as: Mater Sci Eng R Rep. 2015 Mar 1;89:1–48. doi: 10.1016/j.mser.2015.01.002

Figure 13.

Figure 13

Temperature and frequency dependent dielectric behavior of [001]c cut (nonpoled) relaxor-PT single crystals: (a) 0.66PMN-0.34PT; (b) 0.71PMN-0.29PT. ‘Tm shift’ denotes the shift of temperature of the dielectric maximum with frequency from 20 Hz to 1M Hz. Classic and relaxor-like ferroelectric behaviors were observed in 0.66PMN-0.34PT and 0.71PMN-0.29PT single crystals, respectively.