Table 2.
Sample No. | Group Ia | Group IIb |
---|---|---|
1 | 1.4 | 0.0d |
2 | 2.0 | 0.0d |
3 | 1.4 | 0.0d |
4 | 1.9 | 0.1 |
5 | 0.6 | 0.4 |
6 | 2.6 | 0.0d |
7 | 0.7 | 0.0d |
8 | 1.0 | 0.0d |
9 | 0.9 | 0.0d |
10 | 0.7 | 0.0d |
Mean | 1.3 (0.7)c | 0.3 (0.3)c |
Group I = Class-I preparations restored with Z100 (high-shrinkage composite)
Group II= Class-I preparations restored with LS (low-shrinkage composite)
Standard deviation
Where silver nitrate was not found visually the volume of microleakage was assumed to be 0.0 mm3