Skip to main content
. 2014 Dec 8;90(3):573–581. doi: 10.1002/jctb.4589

Table 3.

Macromolecular composition of BSG before and after aqueous ammonia soaking (AAS) pretreatment

Solid compositionb
SRa (%) Lignin (%) Glucan (%) Xylan (%) Arabinan (%)
BSG untreated - 12.8 27.5 28.8 4.32
BSG AAS 59.96 2.09 25.9 23.3 3.26
a

Solid remaining after reaction.

b

Solid percentage composition based on oven dry untreated biomass.