Skip to main content
. 2015 Feb 11;10:56. doi: 10.1186/s11671-015-0732-7

Figure 3.

Figure 3

AFM images of titanium dioxide layer deposition by RF magnetron sputtering at (a) 3 Pa and (b) 5 Pa, without substrate bias, and (c) 3 Pa with a substrate bias of −50 V.