Skip to main content
. 2015 Feb 28;10:90. doi: 10.1186/s11671-015-0810-x

Figure 1.

Figure 1

Ultrasmooth AgNW anode fabricated on photopolymer substrate by spin-coating process and peel-off process. (a) AgNW suspension drop down on Si substrate and spin-coating at 8,000 rpm for 30 s; (b) dry in ambient environment room temperature; (c) NOA63 drop down and spin-coating for first spinning at 300 rpm for 15 s, second spinning at 800 rpm for 15 s; (d) after spin-coating; (e) UV curing at 300 W (370 nm) for 4 min; (f) peel-off process.