Skip to main content
. 2015 Apr 13;10(4):e0123433. doi: 10.1371/journal.pone.0123433

Table 1. Performances of the DSSCs based on ZnO nanorods, nanocons, and heterostructure ZnO–ZnS nanocones.

Cells Jsc (mA/cm2) Voc (V) FF η (%) dye loading (10−8 mol/cm2)
ZnO nanorods 4.9 0.43 0.44 0.93 1.93
ZnO nanocones 8.4 0.54 0.46 2.09 1.58
ZnO-ZnS core-shell nanocones 12.2 0.68 0.49 4.07 3.67