Table 1.

A. Molecular characteristics of π-rich and π-poor CPPMs.

Diester Homopolymers

CPPM Mna Đa
8a 11,600 1.05
8b 11,200 1.05
8c 11,300 1.05
8d 12,600 1.05
8e 11,400 1.05
8f 11,500 1.05
B.

Imide and Diester Random Copolymers

CPPM n:mb Mna Đa
11a 56:44 16,200 1.06
11b 55:45 13,700 1.07
11c 58:42 17,000 1.06
14a 38:62 10,600 1.10
14c 40:60 12,100 1.08
14e 39:61 10,700 1.14
a

Number average molecular weight (Mn) and polydispersity indices (Đ=Mw/Mn) determined by GPC using polymethyl methacrylate (PMMA) standards for diester polymers and polystyrene standards for the imide polymers using tetrahydrofuran (THF) as the eluent and toluene as the flow marker.

b

Ratio of residues, where n represents the percentage of hydrophobic residues and m represents the percentage of guanidine-containing residues.