Skip to main content
. 2015 Mar 27;26(2):71–76. doi: 10.1089/hgtb.2015.040

FIG. 4.

FIG. 4.

Vector materials contact. Serum AAT ELISA results. Significant decrease in the serum levels that contacted stainless steel (p=0.0003), glass (p<0.0001), and polyethylene (p=0.0001) when compared with the polypropylene (PP) control group (n=5).