Skip to main content
. 2015 Jun 6;5(3):20140083. doi: 10.1098/rsfs.2014.0083

Figure 6.

Figure 6.

(a) Linear sweep voltammogram (10 mV s−1) recorded under chopped light on a PS-b-P2VP-templated three-layer NiO film sensitized with 1 in [Co(NH3)5Cl]Cl2 (10 mM)/acetate buffer (pH 4.5; 0.1 M). (b) Cathodic photocurrent measurements recorded on NiO electrodes sensitized with 1 in [Co(NH3)5Cl]Cl2 (10 mM)/acetate buffer (pH 4.5; 0.1 M) with 0 V versus Ag/AgCl applied potential: PS-b-P2VP-templated three-layer NiO film (blue trace) and F108-templated NiO films (one layer: fuchsia trace; two layers: red trace; three layers: green trace).