Table 2.
Characterizing Data on the Electrospinning Fibers Produced
| Fiber ID | Diameter (nm) | Porosity (%) |
|---|---|---|
| PDO | 578±234 | 85.3 |
| PU | 856±198 | 88.5 |
| PHBVV | 606±268 | 86.1 |
| PDO-RGD | 133±28.1 | 84.5 |
Diameters are reported as mean±SD, and porosity has been calculated using the method of Ghasemi-Mobarakeh et al.47