Skip to main content
. 2015 Mar 25;15(4):7206–7227. doi: 10.3390/s150407206

Figure 16.

Figure 16

Deposited SnO2 thickness versus deposition time. The inset shows the dependence of temperature and solution aging on the deposited thickness. A half-day aged solution is used in the given experiment.