Fig. 3. Stress–strain data for SIS30 injection moulded at 7 × 10–8 m3 s–1 into (a) 0.95 mm, (b) 0.45 mm, (c) 0.23 mm thick samples; at 2 × 10–8 m3 s–1 into (d) 0.97 mm, (e) 0.44 mm thick samples; and at 2.8 × 10–8 m3 s–1 into (f) a 0.30 mm thick sample. (g) Schematic of the layout of 0°, 45° and 90° specimens with reference to the disc's radius. P and N represent stress–strain data for unidirectionally oriented samples of SIS30 with cylinders aligned parallel (P) and normal (N) to the stretching direction, respectively.