Skip to main content
. 2015 Mar 15;8(3):3202–3209.

Table 4.

OCN production of osteogenic rMSCs on β-TCP/PLLA composite with different pore size (β-TCP/PLLA = 2:1, porosity =70%) ( ± s, n = 8)

Groups OCN (ng/ml) 7 d OCN (ng/ml) 14 d
d=200-450 µm 3.3 ± 0.29 7.6 ± 0.32
d=450-900 µm 3.1 ± 0.16 6.6 ± 0.30*
*

P < 0.05 vs d = 200-450 µm.