Table 4. Glass forming properties of PG and glycerol VSs with 400μg/ml of AFP during cooling in the liquid nitrogen and warming in the original solution by cryoloop, cryotop and OPS methods.
Solution | Original Solution + 400μg/ml AFP | ||
---|---|---|---|
OPS | Cryotop | Cryoloop | |
Glycerol VS1 | VD | VD | VD |
Glycerol VS2 | VD | VD | VD |
Glycerol VS3 | C | VD | C |
Glycerol VS4 | C | VD | C |
Glycerol VS5 | C | VD | C |
PG VS1 | VV | VV | VV |
PG VS2 | VD | VV | VD |
PG VS3 | VD | VD | VD |
PG VS4 | C | VD | C |
PG VS5 | C | VD | C |
VV—indicates vitrification when cooled as well as when warmed. VD—indicates vitrification when cooled but devitrifies upon thawing. C—indicates crystallization occurs when placed in liquid nitrogen.