Skip to main content
. 2015 May 19;2015:508656. doi: 10.1155/2015/508656

Table 2.

Molecular weight, Mw (g/mol), the polydispersity index, Ip and sulfur content, S (wt%) of GY785 DR and GY785 DRS obtained after sulfation carried out at different temperatures.

Derivative Temp. (°C) Mw- (g/mol) Ip S* (wt%) S** (wt%)
GY785 DR 7,500 1.1 3.4 3.0

GY785 DRS 65 9,000 1.1 8.2 7.6
70 11,000 1.1 9.7 10.4
90 10,500 1.1 11.2 11.1
120 8,000 1.3 10.7 10.1

*Determined by the elemental analysis.

**Determined by HPAEC method.