Figure 2.

Figure 2.

Young’s modulus, E (MPa), plotted against the natural logarithm of the strain rate, loge(ε·), when ε· is measured in s−1, for mixtures with a range of values for the volume fraction, ϕ, of silicone oil: 0 (i.e. pure elastomer), filled circles; 0.11, open circles; 0.33, filled squares; 0.43, open squares; 0.53, filled diamonds; 0.73, open diamonds. Mean values of E are plotted; error bars represent standard deviations.