Skip to main content
. 2015 Jun 15;10(6):e0126047. doi: 10.1371/journal.pone.0126047

Table 1. Chemical composition of the green polyethylene before and after 120 d of exposure to sunlight.

Mineral Composition* Exposure time to sunlight (days)
0 120
Si 41.19 A 35.83 B
Mn 8.51 A 7.41A
Fe 7.74 A 6.73 A
Co 6.31 A 5.49 A
Cu 3.05 A 2.65 A
Zn 8.08 A 7.03 A
Cd 22.06 A 19.19 B
N 2.80 A 2.44 A

* Relative concentration of elements ((weight %) at the surface of the plastic bags, analyzed by scanning electron microscopy coupled to X ray diffraction (semi-quantitative method). Means followed by different letters within the same line differ at Tukey test (P<0.05).