Skip to main content
. 2015 May 6;15(5):10686–10704. doi: 10.3390/s150510686

Figure 5.

Figure 5

Nyquist plots of 220 nm thick bio-modified SnO2 nanoporous film with (a) vapour phase and (b) liquid phase silanization processes. DNA complementary hybridization was performed with target concentration of 2 µM. The filled symbols correspond to experimental data and the continuous lines to fitting data. The inset shows the corresponding typical fluorescence micrograph after hybridization of complementary target labelled with Cy3.