Skip to main content
. Author manuscript; available in PMC: 2015 Jul 1.
Published in final edited form as: Chemistry. 2007;13(15):4138–4144. doi: 10.1002/chem.200700317

Figure 6.

Figure 6

Polystyrene molecules immobilized on silicon wafers. Mw of the monodisperse sample was a) 223 200, b) 570 000, and c) 1877 000. The wafers were treated with PFPA-silane in toluene at the concentration of a) 5 × 10−5 mg mL−1, b) 1 × 10−5 mg mL−1, and c) 5 × 10−6 mg mL−1. The scan area is 1 µm × 1 µm for all images. Adopted from reference [46].