Skip to main content
. 2015 Jun 21;2015:423615. doi: 10.1155/2015/423615

Table 2.

Physicochemical properties of the tablets before and after thermal treatment.

Parameters LCAL LCAD LCA60 LC50A40
Before After Before After Before After Before After
Weight (mg) 422.9 ± 6.1 404.7 ± 2.5 420.8 ± 1.5 397.1 ± 2.0 421.3 ± 1.7 420.8 ± 3.7 418.8 ± 3.9 418.7 ± 6.1
Thickness (mm) 2.99 ± 0.03 3.00 ± 0.01 2.74 ± 0.01 2.77 ± 0.02 2.98 ± 0.01 3.02 ± 0.02 3.47 ± 0.04 3.58 ± 0.07
Diameter (mm) 12.01 ± 0.03 12.06 ± 0.03 12.03 ± 0.05 12.05 ± 0.07 12.04 ± 0.05 12.14 ± 0.04 12.02 ± 0.02 12.09 ± 0.02
Hardness (kP) 8.43 ± 0.43 7.04 ± 0.38 7.35 ± 0.46 6.56 ± 0.46 2.8 ± 0.31 4.02 ± 0.34 4.09 ± 0.62 4.80 ± 0.53
Disintegration (min) 60 ± 0.00 60 ± 0.00 60 ± 0.00 60 ± 0.00 13.00 ± 3.09 31.00 ± 10.52 60 ± 0.00 47.60 ± 11.07
Friability (%) 0.05 0.00 0.06 0.00 11.77 0.07 0.00 0.00

n = 3; data are expressed as mean ± standard deviation. Formulation parameters were evaluated before and after thermal treatment.