Skip to main content
. 2014 Sep 1;2(11):1098–1104. doi: 10.1002/adom.201400327

Figure 6.

Figure 6

(a–c) Optical images of patterned POFs made of SiO2@PMMA@PEA at different stretch ratios up to 25% and (d–f) corresponding reflection spectra in three typical regions. (g) shows tuning of wavelength with strain. Scale bars in (a–c) are 100 μm.