Skip to main content
. 2014 Apr 23;14(Suppl 1):37–45. doi: 10.1007/s13191-014-0359-x

Table 3.

Comparison of microleakage seen in CAD milled and Copy milled samples when cemented using (a) light cure resin bonding system and (b) self cure resin bonding system

Light/self CAD/COPY N Mean Rank Sum of Ranks Mann–Whitney U Wilcoxon W Z P value
Light cured L2/L1 CAD milled 8 10.94 87.5 12.5 48.5 −2.189 0.038
COPY milled 8 6.06 48.5
Self cured L2/L1 CAD milled 8 9.25 74 26 62 -0.631 0.574
COPY milled 8 7.75 62
N Minimum Maximum 25th Percentile MEDIAN 75th IQR
Light cure L2/L1 CAD milled 8 0 0.11 0.0075 0.06 0.09625 0.08875
COPY milled 8 0 0.06 0 0 0.0225 0.0225
Self cure L2/L1 CAD milled 8 0.02 0.6 0.049 0.135 0.2475 0.1985
COPY milled 8 0.02 0.31 0.03125 0.105 0.1775 0.14625