Effect of PEGDTT concentration on the in vitro hydrolytic degradation of PEGDA hydrogels. Changes in hydrogel swelling ratio as a function of incubation time in PBS at 37°C. PEGDA and 0.5 PEGDTT gels were statically similar through 21 days.* Loss of mechanical integrity.