Skip to main content
. 2015 Jul 20;10:4593–4603. doi: 10.2147/IJN.S83788

Figure 9.

Figure 9

The failure-load values of Ti and USP-Ti at 12 weeks after implantation measured by the pull-out test.

Notes: Data are shown as the mean ± SD. *P<0.05 compared with Ti.

Abbreviations: USP-Ti, Ti surface subjected to USP; USP, ultrasonic shot peening; SD, standard deviation; Ti, titanium.