Skip to main content
. 2015 Apr 27;8(12):2123–2132. doi: 10.1002/cssc.201403402

Table 1.

BET specific surface area (SSA), micropore volume (Vm), room-temperature CO2 uptake, and CO2/N2 selectivity of all the nZDCs before and after acid treatment (represented by a and c) and nZIF-8.

Sample SSA Vm CO2 uptake at 25 °C [mmol g−1] SInline graphic
[m2 g−1] [cm3 g−1] 0.15 bar 1.0 bar 20.0 bar
ZIF-8 1700 0.52 0.09 0.70 7.80 11
600a 517 0.15 1.08 2.24 4.77 35
700a 494 0.17 1.01 2.43 4.40 34
800a 616 0.20 1.17 2.78 5.99 30
900a 834 0.29 1.24 3.35 8.16 24
1000a 1292 0.44 1.04 3.31 10.06 18
600c 716 0.25 1.09 2.66 6.48 62
700c 950 0.35 1.40 3.51 7.82 79
800c 922 0.31 1.22 3.27 7.70 29
900c 925 0.34 1.10 3.21 7.80 25
1000c 1222 0.43 0.99 3.22 10.21 22