Skip to main content
. 2014 Aug 22;20(40):12954–12961. doi: 10.1002/chem.201403067

Figure 1.

Figure 1

a) XRD pattern of ZnO nanowire array grown on FTO glass substrate at 90 °C for 4 h. Asterisks indicate peaks of SnO2 (FTO substrate). b) UV/Vis transmittance spectra of ZnO films fabricated at 90 °C for 4 h as a function of precursor concentration. The inset shows the transmittance spectrum of a bare FTO glass substrate.