Skip to main content
. 2014 Aug 22;20(40):12954–12961. doi: 10.1002/chem.201403067

Figure 3.

Figure 3

IV curves measured in a 0.2 m Na2SO4 solution with phosphate buffer (pH 7) for ZnO films synthesized at 90 °C for 4 h with varying precursor concentration.