Figure 2. FT-IR spectrum of ZnAl2O4 nanoparticles prepared from (S1) Al2(SO4)3∙18H2O, (S2) AlCl3∙6H2O, and (S3) Al(NO3)3∙9H2O and sintered at 600 °C.