. 2015 Aug 4;5:12849. doi: 10.1038/srep12849

Figure 5. SEM images and particle size distribution of ZnAl2O4 xerogel prepared from (S1) Al2(SO4)3∙18H2O, (S2) AlCl3∙6H2O, and (S3) Al(NO3)3∙9H2O and sintered at 700 °C.

Figure 5