. 2015 Aug 4;5:12849. doi: 10.1038/srep12849

Figure 6. (S1–S3) TEM image, (SH1- SH3) HRTEM image, and (SP1–SP3) Particle size distribution of ZnAl2O4 nanoparticles prepared from (S1) Al2(SO4)3∙18H2O, (S2) AlCl3∙6H2O, and (S3) Al(NO3)3∙9H2O and sintered at 700 °C.

Figure 6

The inset presents the SAED pattern taken from a portion of the ZnAl2O4 nanoparticles shown in Fig. 6(S2).