Skip to main content
. 2015 Jul 14;31(30):8386–8391. doi: 10.1021/acs.langmuir.5b00936

Figure 3.

Figure 3

Neutron reflectivity profiles for DMPC/DMPG-MSP1E3D1 after 6 h incubation time at 14 °C, and upon heating the film to 38 °C and recooling to 14 °C. The SLD for the best fits (inset) show that the nanodisc film becomes thinner and increases in coverage upon heating, and this effect is semireversible. For clarity, in the latter case only the D2O contrast is shown. Typical SiO2 layers were 5 ± 1 Å thick with 3 ± 1 Å roughness.