Skip to main content
. 2015 Jul 27;2015:502820. doi: 10.1155/2015/502820

Table 3.

Shear strengths of the metal-bone cement interfaces (MPa) before immersion and 4 weeks after immersion in each group.

Group Before immersion 4 weeks after immersion P #
G0 5.746 ± 0.7701 4.244 ± 0.0709 <0.05
G1 5.668 ± 0.0864 4.200 ± 0.0632 <0.05
G2 5.652 ± 0.0834 4.178 ± 0.0581 <0.05
G3 5.598 ± 0.1188 4.172 ± 0.0286 <0.05
G4 5.564 ± 0.1250 4.138 ± 0.0835 <0.05
G5 5.534 ± 0.1043 3.530 ± 0.0418* <0.05
P ## 0.053 <0.05

Note: ##indicates one-way analysis of variance (ANOVA); #indicates t-test, P < 0.05; *indicates Scheffé's post hoc test, P < 0.05 compared with G0.