Figure 1.
Dependence of the conversion on the time for the copolymerization of AOMEC (nAOMEC/nBn–OH = 100) and εCL (nεCL/nBn–OH = 100). Solution polymerizations at −40 (top left) and +30 °C (top right) were performed in dry DCM (2 M to nAOMEC + nεCL). At 100 (bottom left) and 170 °C (bottom right), the polymerizations were performed in bulk. All of the polymerizations were conducted with TBD (nTBD/nBn–OH = 2.5) as the catalyst.