Table 1. Experimental groups depending on the fabrication system and finish line configuration used in this study.

Fabrication system Composition Finish line configuration
IPS e.max®press
(IvoclarVivadent AG,Schaan, Liechtenstein)
Lithium disilicate glass-ceramic Deep chamfer (n=8)
Shoulder (n=8)
Prettau®Zirconia
(Zirkonzahn GmbH; Gais, Italy)
Presintered yttrium stabilized zirconium dioxide Deep chamfer (n=8)
Shoulder (n=8)
ZENOSTAR®ZR translucent
(Wieland Dental GmbH, Pforzheim, Germany)
Deep chamfer (n=8)
Shoulder (n=8)