Table 2.
Root-mean-square (RMS) roughness measurements of HNT and NaL-HNT using atomic force microscopy. Data are mean ± standard deviation of three independent measurements.
| Sample | RMS Roughness (nm) |
|---|---|
| HNT | 163.14 +/− 34.52 |
| NaL-HNT | 132.31 +/− 48.47 |
Root-mean-square (RMS) roughness measurements of HNT and NaL-HNT using atomic force microscopy. Data are mean ± standard deviation of three independent measurements.
| Sample | RMS Roughness (nm) |
|---|---|
| HNT | 163.14 +/− 34.52 |
| NaL-HNT | 132.31 +/− 48.47 |