Skip to main content
. 2015 Jun 2;104(8):2513–2522. doi: 10.1002/jps.24503

Figure 5.

Figure 5

Histogram of tablet coating thicknesses inside the coating pan from 80 to 320 min where the mixing baffles were removed after 200 min. The large thickness values (>150 μm) acquired do not represent reliable measurements and are artefacts because of relaxed acceptance criteria.