Skip to main content
. 2015 Sep 3;5:12914. doi: 10.1038/srep12914

Figure 2.

Figure 2

SEM images of ZnO-250 (a), ZnO:20%Zn (b) and ZnO-900 samples (c). TEM micrographs of ZnO-250 (d), (e). Inset in (e) is the corresponding FFT. Spots and [100] zone axis were identified with the stoechiometric ZnO structure (ICSD file: 162843). (f) Top: simulated image (thickness 3.25 nm, defocus 30 nm), bottom: experimental micrograph.