Figure 1. Changes in rubber latex parameters after different treatments.

Figure 1

The fresh yield (a), dry matter (b), water content (c) and flow time (d) for latex collected from rubber trees treated with ethylene (3% ethephon, marked with black rectangle) and ddH2O (white) for 0, 3 and 5 days are presented. Total rubber particles from untreated plants (e, day 0) and plants treated with ddH2O (f) and ethylene (g) for 3 days were examined under SEM.