Figure 7. Effect of GO flake size (a,b) and heat treatment temperature (c,d) on the compressive modulus and the yield stress of the porous networks.

Figure 7

In (a,b), data points from the small flake samples are shadowed. In (c) and (d), the densities of the tested samples are all ∼5 mg/cm3. In order to keep similar GO concentration in the starting solution, the unreduced GO-PN samples were produced without the addition of the binder.