XPS titanium and sulfur composition vs CuBr2 per nominal cm2 of initiator-functionalized surface area for both replicates (A). AFM measured thicknesses vs CuBr2 per nominal cm2 of initiator-functionalized surface for both replicates (B). For both panels, data from replicate 1 and 2 are represented by closed and open symbols, respectively. These results show that NaSS film thickness decreases with increasing catalyst amount.