Fig. 4.

Fig. 4

Optical micrographs of urea–formaldehyde-(UF) bond lines. Two different adhesives were applied, once without any additional filler (UF-1 and UF-2) and once filled with 2 wt% fibrillated pulp (P1). Adhesive spread was 250 g/m² of solid resin in all cases