Skip to main content
. Author manuscript; available in PMC: 2016 Nov 1.
Published in final edited form as: J Mech Behav Biomed Mater. 2015 Aug 1;51:345–355. doi: 10.1016/j.jmbbm.2015.07.027

Table 2.

Median fatigue life (Nf) based on 1% creep failure definition, at maximum stress applied (σmax). Values reported as ‘median (n=6), (25% percentile, 75% percentile).’ ‘-’ indicates the specimen was not subjected to corresponding stress. Mann-Whitney tests were performed to determine statistical significance between the mean of groups.

σmax (MPa) PCL-BG/PUR CaS/P U-BG/PUR
5 230500a (66500, 495000) 23500 (12500, 36750) 3 (2, 3) ab
10 38000a (20250, 52000) 236 (70, 511) -
15 58500a (24500, 69250) 4 (3, 16) -
20 9075 (5960, 15735) - -
25 710 (327, 2443) - -
30 1115 (383, 1458) - -
a

p<.0022, at specific σmax relative to to CaS/P.

b

p<.0022, at specific σmax relative to to PCL-BG/PUR.